Material Notes:
Product Description: A homopolymer resin designed for injection molding applications requiring excellent flow and good mechanical properties. It is designed for caps and closures, general applications such as toys, electric appliances, packaging and thin walled parts.Availability: Africa & Middle East and Asia Pacific Uses: Consumer ApplicationsCratesFurniture Industrial Applications PackagingTool/Tote Box Processing Method: Compounding and Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ISO 868
Tensile Strength, Yield 33.0 MPa
4790 psi
ISO 527-2/1A/50
Elongation at Yield 9.0 %
9.0 %
ISO 527-2/1A/50
Tensile Modulus 1.42 GPa
206 ksi
ISO527-2/1A/1
Flexural Modulus 1.33 GPa
193 ksi
0.079 in/min; ISO 178
Charpy Impact, Notched 0.336 J/cm²
1.60 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 318 °C
604 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 78.9 °C
174 °F
ISO 75-2/B