Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.336 J/cm² @Temperature 22.8 °C |
1.60 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ HMU 210 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness for automotive HVAC and under-the-hood applications.Availability: Africa & Middle East, Asia Pacif.. |
|||
Charpy Impact, Notched | 0.336 J/cm² @Temperature 22.8 °C |
1.60 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ HMU 234 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness, high heat stabilization, low emissions and low odor for automotive HVAC and under-the-hood applic.. |
|||
Charpy Impact, Notched | 0.336 J/cm² | 1.60 ft-lb/in² | ISO 179/1eA |
ExxonMobil PP1304E3 Polypropylene Copolymer Product Description: A homopolymer resin designed for injection molding applications requiring excellent flow and good mechanical properties. It is designed for caps and closures, general applicati.. |