Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 193 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.33 GPa
193 ksi
Tangent; 1.3 mm/min; ISO 178
Mytex Polymers AS33L-07VS Polypropylene, Rubber modified, Compounded
Description: AS33L-07 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key..
Flexural Modulus 1.33 GPa
193 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS
LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic.
Flexural Modulus 1.33 GPa
193 ksi
ASTM D790
Styrolution Styrolux® 3G46 SBC
Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im..
Flexural Modulus 1.33 GPa
193 ksi
ASTM D790
Total HDPE BM961 High Density Polyethylene, High Gloss Blow Molding Resin
Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p..
Flexural Modulus 1.33 GPa
193 ksi
0.079 in/min; ISO 178
ExxonMobil PP1304E3 Polypropylene Copolymer
Product Description: A homopolymer resin designed for injection molding applications requiring excellent flow and good mechanical properties. It is designed for caps and closures, general applicati..
Flexural Modulus 1.33 GPa
193 ksi
.5"/min; CP-TM-10
PolyOne Elastamax HTE 2101-1000 Polyurethane Alloy  (discontinued **)
This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. ..