Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.33 GPa | 193 ksi | Tangent; 1.3 mm/min; ISO 178 |
Mytex Polymers AS33L-07VS Polypropylene, Rubber modified, Compounded Description: AS33L-07 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key.. |
|||
Flexural Modulus | 1.33 GPa | 193 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Flexural Modulus | 1.33 GPa | 193 ksi | ASTM D790 |
Styrolution Styrolux® 3G46 SBC Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im.. |
|||
Flexural Modulus | 1.33 GPa | 193 ksi | ASTM D790 |
Total HDPE BM961 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Flexural Modulus | 1.33 GPa | 193 ksi | 0.079 in/min; ISO 178 |
ExxonMobil PP1304E3 Polypropylene Copolymer Product Description: A homopolymer resin designed for injection molding applications requiring excellent flow and good mechanical properties. It is designed for caps and closures, general applicati.. |
|||
Flexural Modulus | 1.33 GPa | 193 ksi | .5"/min; CP-TM-10 |
PolyOne Elastamax HTE 2101-1000 Polyurethane Alloy
(discontinued **) This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. .. |