ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast. Availability: Latin America, North America and South America Additive: Antiblock: 6000 ppmSlip: 1500 ppmProcessing Aid: Yes Thermal Stabilizer: YesApplications: Blown FilmBread BagsCast FilmFood packagingPackaging FilmsPaper OverwrapZipper BagInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ExxonMobil method
Melt Flow 3.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 6000 ppm
6000 ppm
Slip Level 1500 ppm
1500 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.3 MPa
1500 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa
1500 psi
ASTM D882
Film Elongation at Break, MD 610 %
610 %
ASTM D882
Film Elongation at Break, TD 850 %
850 %
ASTM D882
Puncture Energy 1.58 J
1.17 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 20 g
20 g
ASTM D1922
Elmendorf Tear Strength TD 300 g
300 g
ASTM D1922
Dart Drop Test <= 50.0 g
<= 0.110 lb
ASTM D1709A
Film Tensile Strength at Break, MD 44.8 MPa
6500 psi
ASTM D882
Film Tensile Strength at Break, TD 24.1 MPa
3500 psi
ASTM D882
1% Secant Modulus, MD 200 MPa
29000 psi
ASTM D882
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 253 °C
<= 487 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 1.1 %
1.1 %
ASTM D1003
Gloss 92 %
92 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 7 lbf
ExxonMobil Method