Mechanical Properties Metric English Comments
1% Secant Modulus, TD 214 MPa
31000 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE  (discontinued **)
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a..
1% Secant Modulus, TD 214 MPa
31000 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE  (discontinued **)
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a..
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D882
Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D882
Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization packageCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use stra..
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D882
Westlake LF1040 Butene Linear Low Density Polyethylene
Westlake LF1040 is a butene LLDPE resin with excellent mechanical and sealing properties. It can be used in stretch film and can liner applications, and is suitable for blending with LDPE in packagi..
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D882
Chevron Phillips MarFlex® 7120B LLDPE Blown & Cast Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D882
Chevron Phillips MarFlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film
This LLDPE is tailored for cast film applications that require:Good stiffness at thin gaugesGood drawdownExcellent processabilityCan be used singly or in blends with LDPE or HDPEAvailable with slip ..
1% Secant Modulus, TD 214 MPa
31000 psi
Cast Film at 1.25 mil; ASTM D-882
Chevron Phillips MarFlex® 7120X Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L..
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D882
ExxonMobil LLDPE LL 1236.85 Linear Low Density Polyethylene Resin
Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast...
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D882
ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin
Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast...
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D882
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b..
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D-882
Bapolene® 200B Polyethylene, Film Extrusion
Bapolene 200B is a low density polyethylene for blown film applications requiring superior clarity. It complies with US FDA 21CFR177.1520.Applications: General purpose, bakery, flexible, medical an..