Material Notes:
Product Description: Exact 3040 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monoextrusion and coextrusion coating applications. It offers outstanding adhesion and very low seal initiation temperature combined with high hot tack and seal strengths. This grade is specially recommended for enlarging the sealing window and to seal through contamination. It can be used as a minority or majority component in LDPE to improve optical and sealing performance.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoProcessing Aid: NoThermal Stabilizer: NoApplications:Extrusion CoatingExtrusion LaminationNon-woven Coating Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 17 g/10 min
17 g/10 min
ExxonMobil Method
Neck In 4.83 cm
1.90 in
328 ft/min, Blend with 40% LDPE, Constant output at 35 rpm; ExxonMobil Method
4.83 cm
1.90 in
656 ft/min, Blend with 40% LDPE, Constant output at 35 rpm; ExxonMobil Method
6.86 cm
2.70 in
656 ft/min, Blend with 20% LDPE, Constant output at 35 rpm; ExxonMobil Method
7.87 cm
3.10 in
328 ft/min, Blend with 20% LDPE, Constant output at 35 rpm; ExxonMobil Method
Drawdown 5.16 m/s
1020 ft/min
Blend with 40% LDPE, Constant output at 35 rpm; ExxonMobil Method
6.16 m/s
1210 ft/min
Blend with 40% LDPE, Constant output at 65 rpm; ExxonMobil Method
>= 10.0 m/s
>= 1970 ft/min
Blend with 20% LDPE, Constant output at 35 rpm; ExxonMobil Method
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 77.2 °C
171 °F
ASTM D1525