Polymer Property : Vicat Softening Point = 77.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 77.2 °C
171 °F
ASTM D1525
Teknor Apex Sinvicomp SBB 3616 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P..
Vicat Softening Point 77.2 °C
171 °F
ASTM D1525
Teknor Apex Sinvicomp SBB 3715 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P..
Vicat Softening Point 77.2 °C
171 °F
120°C/hr, 9.8N; ASTM D1525
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Memory and elasticity, Impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane pro..
Vicat Softening Point 77.2 °C
171 °F
ASTM D1525
ExxonMobil Escorene® LD 705.MJ Molding, extrusion and compounding resin
Escorene Ultra LD 705.MJ is a fraction melt index, 13.3 wt% vinyl acetate copolymer suitable for use in making blow molded articles, extruded profiles and compounds.Information provided by ExxonMobi..
Vicat Softening Point 77.2 °C
171 °F
ASTM D1525
ExxonMobil Exact™ 3040 Cast Ethylene-based Plastomer Resin
Product Description: Exact 3040 is an ethylene-based hexane copolymer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monolayer and coextrusion cast fi..
Vicat Softening Point 77.2 °C
171 °F
ASTM D1525
ExxonMobil EXACT™ 3040 Plastomer for Extrusion Coating Applications
Product Description: Exact 3040 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monoextrusion and coextrusion coa..
Vicat Softening Point 77.2 °C
171 °F
ASTM D1525
Teknor Apex Sinvicomp SBB 3615 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provide..
Vicat Softening Point 77.2 °C
171 °F
ASTM D1525
ExxonMobil Escorene™ LD 705.MJ Blown Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 705.MJ is a fractional melt index, 12.8 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and..