Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 4.83 cm | 1.90 in | 328 ft/min, Blend with 40% LDPE, Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil EXACT™ 3040 Plastomer for Extrusion Coating Applications Product Description: Exact 3040 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monoextrusion and coextrusion coa.. |
|||
Neck In | 4.83 cm | 1.90 in | 656 ft/min, Blend with 40% LDPE, Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil EXACT™ 3040 Plastomer for Extrusion Coating Applications Product Description: Exact 3040 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monoextrusion and coextrusion coa.. |