Physical Properties Metric English Comments
Drawdown 6.16 m/s
1210 ft/min
Blend with 40% LDPE, Constant output at 65 rpm; ExxonMobil Method
ExxonMobil EXACT™ 3040 Plastomer for Extrusion Coating Applications
Product Description: Exact 3040 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monoextrusion and coextrusion coa..