Material Notes:
Staramide Z1000XXC is an UV Stabilized Polyamide 66 Injection Molding Resin (also known as R1000HI0944)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm
0.016 - 0.018 in/in
on Tensile Bar; E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 MPa
7110 psi
5 mm/min; ISO 527
Elongation at Break >= 25 %
>= 25 %
5 mm/min; ISO 527
Flexural Strength 63.0 MPa
9140 psi
2 mm/min; ISO 178
Flexural Modulus 1.70 GPa
247 ksi
2 mm/min; ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 89.0 °C
>= 192 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af