Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurofoam Evacell XM 2001 EVA + PE Foam

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Polyethylene (PE)
Manufacturer Eurofoam s.r.l.
Trade Name Evacell
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Evacell XM 2001 EVA + PE Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, dielectric properties and good insulating properties. It is resistant to UVA radiation. It can be silk-screened and thermoformed.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.0450 - 0.0650 g/cc
0.00163 - 0.00235 lb/in³
ISO 845-88
Water Absorption <= 5.0 %
<= 5.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 55 - 65
55 - 65
ASTM D 2240
Tensile Strength 0.400 MPa
58.0 psi
ASTM D 412
Elongation at Break >= 150 %
>= 150 %
ASTM D 412
Compressive Yield Strength 0.0700 MPa

@Strain 25.0 %
10.2 psi

@Strain 25.0 %
ASTM 1056/85
0.150 MPa

@Strain 50.0 %
21.8 psi

@Strain 50.0 %
ASTM 1056/85
Tear Strength 0.240 kN/m
1.37 pli
ASTM D 624
Compression Set 16 %

@Strain 25.0 %
16 %

@Strain 25.0 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
ASTM D 3575
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
ASTM D 3575
Descriptive Properties Value Comments
Cellular Structure Closed
Color Grey
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Fire Resistance MV22 302
Pass
Users viewing this material also viewed the following: