Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0450 - 0.0650 g/cc | 0.00163 - 0.00235 lb/in³ | ISO 845-88 |
Eurofoam Evacell XM 2001 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Density | 0.0550 - 0.0650 g/cc | 0.00199 - 0.00235 lb/in³ | |
Akzo Nobel Expancel® 051 DE 40 d60 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0550 - 0.0650 g/cc | 0.00199 - 0.00235 lb/in³ | |
Akzo Nobel Expancel® 461 DE 40 d60 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0550 - 0.0650 g/cc | 0.00199 - 0.00235 lb/in³ | |
Akzo Nobel Expancel® 551 DE 20 d60 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0180 - 0.0650 g/cc | 0.000650 - 0.00235 lb/in³ | |
BASF Styropor® BFL 422 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |