Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0700 MPa @Strain 40.0 % |
10.2 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Evazote® VA25 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Compressive Yield Strength | 0.0700 MPa @Strain 25.0 % |
10.2 psi @Strain 25.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.0700 MPa @Strain 25.0 % |
10.2 psi @Strain 25.0 % |
ASTM 1056/85 |
Eurofoam Evacell XM 2001 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Compressive Yield Strength | 0.0700 MPa @Strain 50.0 % |
10.2 psi @Strain 50.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 304 CM-RS EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Compressive Yield Strength | 0.0700 MPa @Strain 50.0 % |
10.2 psi @Strain 50.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 304 CM EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Compressive Yield Strength | 0.0700 MPa @Strain 50.0 % |
10.2 psi @Strain 50.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 304 CM-BI EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Compressive Yield Strength | 0.0700 MPa @Strain 50.0 % |
10.2 psi @Strain 50.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 304 CM-GR EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |