Ensinger PVC Polyvinylchloride (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Ensinger
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger PVC Polyvinylchloride (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger's type 1 grey PVC ROD is designed for machining solutions and is a cost effective solution for general industrial applications. The material offers an excellent combination of chemical resistance and mechanical strength, along with good thermal and electrical properties that are suited to a variety of industries.Excellent chemical and corrosion resistanceVery good mechanical strengthNon-contamination for applications requiring high levels of material purityExcellent flammability characteristicsManufactured in rod, Ensinger PVC can be used for applications such as pump housings, valve components and other parts as well as couplings in electronics applications that require good chemical resistance.Information provided by Ensinger
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.3 MPa
7300 psi
ASTM D638
Tensile Modulus 2.83 GPa
410 ksi
ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 2.90 GPa
420 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 52.2 µm/m-°C
29.0 µin/in-°F
ASTM D696
Maximum Service Temperature, Air 60.0 °C
140 °F
long term
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648
Flammability, UL94 V-0
V-0
ASTM D648