Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 52.2 µm/m-°C @Temperature -18.0 - 38.0 °C |
29.0 µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
Plaskolite Optix® Acrylic Sheet Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,.. |
|||
CTE, linear | 52.2 µm/m-°C | 29.0 µin/in-°F | ASTM D696 |
Quantum PPS Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 52.2 µm/m-°C @Temperature 20.0 °C |
29.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum Information provided by ITW Devcon |
|||
CTE, linear | 52.2 µm/m-°C | 29.0 µin/in-°F | ASTM D696 |
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi.. |
|||
CTE, linear | 52.2 µm/m-°C | 29.0 µin/in-°F | |
Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machinin.. |
|||
CTE, linear | 52.2 µm/m-°C | 29.0 µin/in-°F | ASTM D696 |
Ensinger PVC Polyvinylchloride (PVC) Ensinger's type 1 grey PVC ROD is designed for machining solutions and is a cost effective solution for general industrial applications. The material offers an excellent combination of chemical resi.. |
|||
CTE, linear | 52.2 µm/m-°C | 29.0 µin/in-°F | |
BCC Products MB 3500 Urethane Fixture Board MB 3500 is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly sha.. |
|||
CTE, linear | 52.2 - 100 µm/m-°C | 29.0 - 55.6 µin/in-°F | Average value: 70.1 µm/m-°C Grade Count:4 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
CTE, linear | 52.2 - 101 µm/m-°C | 29.0 - 56.0 µin/in-°F | Average value: 75.7 µm/m-°C Grade Count:14 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |