Material Notes:
Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead for weighting, balancing and vibration dampening applicationsInformation provided by Technical Polymers.
Physical Properties Metric English Comments
Specific Gravity 2.50 g/cc
2.50 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 220 %
220 %
ASTM D638
Tensile Modulus 0.552 GPa
80.0 ksi
ASTM D638
Flexural Strength 44.1 MPa
6400 psi
ASTM D790
Flexural Modulus 0.169 GPa
24.5 ksi
ASTM D790
Izod Impact, Notched 2.46 J/cm
4.60 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 204 - 221 °C
400 - 430 °F
Mold Temperature 10.0 - 26.7 °C
50.0 - 80.0 °F
Drying Temperature 82.2 °C
180 °F
do not over dry
Dry Time 2 hour
2 hour