Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.552 GPa @Temperature 22.8 °C |
80.0 ksi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP TIVAR® 1000 Virgin (Natural & Color except Black) UHMW-PE |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet) Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM.. |
|||
Tensile Modulus | 0.552 - 0.896 GPa | 80.0 - 130 ksi | ASTM D638 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Tensile Modulus | 0.552 - 0.896 GPa | 80.0 - 130 ksi | ASTM D638 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.002" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.003" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.005" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.006" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.015" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.031" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.062" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.125" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.250" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.001" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.010" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D-882 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.188" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D638 |
ScanTube PTFE Tubing Information provided by ScanTube, Inc. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D638 |
Lubrizol ESTALOC® 60155 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D638 |
Ecomass® 4703BI74 Filled Polyurethane, Injection Molding Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, radiation shielding applicationsInfor.. |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D638 |
Ecomass® 4703ZC57 Stainless Steel Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Tensile Modulus | 0.552 GPa | 80.0 ksi | ASTM D638 |
Ecomass® 4710BI71 Filled Polyurethane, Injection Molding Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead for weighting, balancing and vibration.. |
|||
Tensile Modulus | 0.552 GPa @Temperature 110 °C |
80.1 ksi @Temperature 230 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi.. |