EPICHEM PA 6/66 GF 30 Polyamide 6/66, 30% Glass

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer EPICHEM srl
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EPICHEM PA 6/66 GF 30 Polyamide 6/66, 30% Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: 30% glass fibre filled
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792, ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 135 MPa
19600 psi
ASTM D638, ISO R527
Flexural Strength 200 MPa
29000 psi
ASTM D790, ISO 178
Izod Impact, Notched 0.550 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.03 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
ASTM D648, ISO 75