Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers Tekaloy® G70F2 G70NH, Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKALOY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers Tekaloy® G70F2 G70NH, Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
V-2, High FlowInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 250 °C
15 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 28 %
28 %
ASTM D638
Flexural Yield Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C
201 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Processing Temperature 210 - 260 °C
410 - 500 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F