Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dynasol Solprene® 4318 Thermoplastic Rubber SBS Dry

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Dynasol
Trade Name Solprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Solprene® 4318 Thermoplastic Rubber SBS Dry.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solprene 4318 is a linear block copolymer of styrene and butadiene, having 32% of styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a non-staining antioxidant system; FDA approved for use in food contact applications and is essentially gel free with a very clear color. S-4318 is used as compounding ingredient for adhesives. The product is an excellent modifier for asphalt applications including self-adhesive roofing membrane and sealant. Also is used in thermoplastic injected shoe soles formulations. It is presented as free flowing porous crumb making easy its handling and dissolution.Applications:Roofing & Plastic modificationAdhesivesInformation provided by Dynasol
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D-5668
Brookfield Viscosity 700 cP
700 cP
25% toluene solution; MA 04-3-064
Viscosity Measure 7.0 cSt
7.0 cSt
Toluene solution viscosity 5,23%; NM 300-11
Melt Index of Compound 8.0 g/10 min
8.0 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
ASTM D-2240
Tensile Strength at Break 3.70 MPa
537 psi
ASTM D-412
Elongation at Break >= 1000 %
>= 1000 %
ASTM D-412
300% Modulus 0.00120 GPa
0.174 ksi
ASTM D-412
Chemical Properties Metric English Comments
Styrene Content >= 31 %
>= 31 %
Block; NM 202-07
32 %
32 %
on polymer; ASTM D-5775