Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.70 MPa @Temperature 23.0 °C |
537 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Tensile Strength at Break | 3.70 MPa | 537 psi | ISO 37 |
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Extrusion, Pebble Gray Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Tensile Strength at Break | 3.70 MPa | 537 psi | ISO 37 |
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Injection Molding, Pebble Gray Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tensile Strength at Break | 3.70 MPa | 537 psi | ASTM D-412 |
Dynasol Solprene® 4318 Thermoplastic Rubber SBS Dry Solprene 4318 is a linear block copolymer of styrene and butadiene, having 32% of styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a .. |
|||
Tensile Strength at Break | 3.70 MPa | 537 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX E 45.1 TPE-V, Shore A45 TPE-VInformation provided by BARLOG plastics GmbH. |