Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 700 cP | 700 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 6020 SBR Latex Applications: Rovene® 6020 is a soft, carboxylated stryene-acrylic copolymer emulsion. The typical films are soft and strong with good water resistance and exhibit good resistance to discoloratio.. |
|||
Brookfield Viscosity | 700 - 1100 cP | 700 - 1100 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1160 B (SIS) Linear Triblock Copolymer Description: Kraton D1160 B is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from South America in the physical form identified: Kr.. |
|||
Brookfield Viscosity | 700 cP @Temperature 190 °C |
700 cP @Temperature 374 °F |
ASTM D3226 |
Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer Product Description: Epolene N-15 is a low viscosity polypropylene homopolymer with a high melt point and excellent hardness. Epolene N-15 is used in color concentrates, toner compounds, and as a pi.. |
|||
Brookfield Viscosity | 700 cP @Temperature 190 °C |
700 cP @Temperature 374 °F |
|
Westlake Epolene® N-15P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-15P is a low viscosity polypropylene homopolymer powder with a high melt point and excellent hardness. Epolene N-15P is used in color concentrates, toner compounds, and as a p.. |
|||
Brookfield Viscosity | 700 cP @Temperature 125 °C |
700 cP @Temperature 257 °F |
|
Westlake Epolene® N-35 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-35 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Brookfield Viscosity | 700 cP | 700 cP | 25% toluene solution; MA 04-3-064 |
Dynasol Solprene® 4318 Thermoplastic Rubber SBS Dry Solprene 4318 is a linear block copolymer of styrene and butadiene, having 32% of styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a .. |
|||
Brookfield Viscosity | 700 - 900 cP @Temperature 25.0 °C |
700 - 900 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 102 Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 102: Resin suitable .. |
|||
Brookfield Viscosity | 700 - 900 cP @Temperature 25.0 °C |
700 - 900 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 106 Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 106: Resin for varni.. |
|||
Brookfield Viscosity | 700 - 900 cP @Temperature 25.0 °C |
700 - 900 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 901 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 901: General purpose.. |