Material Notes:
Melinex® 565 is a high clarity film which is differentially coated. One surface is coated with the standard T-Sub adhesion promoter; the opposite surface is coated for antistatic protection.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 82.7 MPa
12000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 75.8 MPa
11000 psi
ASTM D882A
Film Elongation at Break, MD 150 %
150 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Coefficient of Friction, Static 0.40 - 0.50
0.40 - 0.50
ASTM D1894
Film Tensile Strength at Break, MD 138 MPa
20000 psi
ASTM D882A
Film Tensile Strength at Break, TD 138 MPa
20000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.0e+11 ohm

@Temperature 25.0 °C
1.0e+11 ohm

@Temperature 77.0 °F
500 V DC @ 60% RH; ASTM D257