Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.0e+11 ohm | >= 1.0e+11 ohm | IEC 60093 |
Quadrant EPP Nylatron® MD PA 6 + metal detectable additive, extruded (ISO Data) Metal detectable 6SA grade High wear and fatigue resistance Lower moisture absorption than standard PA6 Metal and visual detection by blue colour Detection by x-ray also possible Continuous use temp.. |
|||
Surface Resistivity per Square | 1.0e+11 ohm @Temperature 25.0 °C |
1.0e+11 ohm @Temperature 77.0 °F |
500 V DC @ 60% RH; ASTM D257 |
DuPont Teijin Films Melinex® 565 Polyester Film Melinex® 565 is a high clarity film which is differentially coated. One surface is coated with the standard T-Sub adhesion promoter; the opposite surface is coated for antistatic protection.Informa.. |