Material Notes:
Ultra Ethylux is made from high density polyethylene resin. This material is a cost effective alternative for a variety of end uses including mild chemical and wear applications. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Elongation at Break >= 700 %
>= 700 %
ASTM D638
Tensile Modulus 0.938 GPa
136 ksi
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 1.71 - 2.40 J/cm
3.20 - 4.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 126 - 198 µm/m-°C

@Temperature 20.0 °C
70.0 - 110 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 127 °C
260 °F
ASTM D4591
Maximum Service Temperature, Air 98.9 °C
210 °F
Continuous Use
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 2.3

@Frequency 1000 Hz
2.3

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.7 kV/mm
475 kV/in
ASTM D149