Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 75.8 MPa | 11000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 565 Polyester Film Melinex® 565 is a high clarity film which is differentially coated. One surface is coated with the standard T-Sub adhesion promoter; the opposite surface is coated for antistatic protection.Informa.. |