Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Surlyn® 1652SR Zinc Ionomer Resin for Cast Film and Extrusion Coating

Category Polymer , Film , Thermoplastic , Ionomer , Ionomer, Film Grade
Manufacturer DuPont
Trade Name Surlyn®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Surlyn® 1652SR Zinc Ionomer Resin for Cast Film and Extrusion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surlyn® 1652SR is an ionomer resin available for use in cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Medical/pharmaceutical packaging; Powdered/granular food and nonfood pouches; Snack structuresData provided by the manufacturer, DuPont Packaging.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 5.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Seal Strength <= 2500 g/25 mm
<= 2500 g/in
Varies with seal bar temp.
Hot Tack Strength <= 2600 g/25 mm
<= 2600 g/in
Varies with seal bar temp.; Packforsk Method
Thermal Properties Metric English Comments
Melting Point 100 °C
212 °F
DSC; ASTM D3418
Vicat Softening Point 79.0 °C
174 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 304 °C
579 °F