Polymer Property : Melt Temperature = 579 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 304 - 332 °C
579 - 630 °F
PolyOne LubriOne™ PC-20CF/15T Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Melt Temperature 304 - 332 °C
579 - 630 °F
PolyOne Therma-Tech™ SF-4500 TC Polyphenylene Sulfide (PPS)
Information provided by PolyOne
Melt Temperature 304 - 332 °C
579 - 630 °F
PolyOne Edgetek® SF2-40CF/000 NATURAL Polyphenylene Sulfide (PPS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Temperature 304 - 332 °C
579 - 630 °F
PolyOne Edgetek® SF-40CF/000 Polyphenylene Sulfide (PPS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Temperature 304 - 343 °C
579 - 649 °F
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Melt Temperature 304 - 343 °C
579 - 649 °F
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Melt Temperature 304 - 343 °C
579 - 649 °F
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Melt Temperature 304 - 343 °C
579 - 649 °F
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Melt Temperature 304 - 332 °C
579 - 630 °F
PolyOne LubriOne™ PC-30CF/20T Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Melt Temperature 304 - 332 °C
579 - 630 °F
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement  (discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
Melt Temperature 304 - 332 °C
579 - 630 °F
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement  (discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
Melt Temperature 304 - 321 °C
579 - 610 °F
NOVA Chemicals Sclair® 69A HDPE Extrusion Resin  (discontinued **)
Features: High tensile strength, better moisture barrier, better oil and solvent resistance, lower friction coefficient, lower brittleness temperature, better abrasion resistance, better temperature..
Melt Temperature 304 °C
579 °F
DuPont™ Surlyn® 1605SBR Sodium Ionomer Resin for Extrusion Coating  (discontinued **)
Surlyn® 1605SBR is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceuti..
Melt Temperature 304 °C
579 °F
DuPont™ Surlyn® 1652SR Zinc Ionomer Resin for Cast Film and Extrusion Coating
Surlyn® 1652SR is an ionomer resin available for use in cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resi..
Melt Temperature 304 - 343 °C
579 - 649 °F
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Melt Temperature 304 - 343 °C
579 - 649 °F
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Melt Temperature 304 - 321 °C
579 - 610 °F
LNP Thermocomp® SPS-F-1006 HS Syndiotactic Polystyrene, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..