Material Notes:
DuPont™ Elvax® 466 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 466 resins can be used for the following applications: adhesives, sealants, and wax blends.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ASTM D792-ISO 1183
Vinyl Acetate Content 18 %
18 %
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
ASTM D2240-ISO 868
Hardness, Shore D 41
41
ASTM D2240-ISO 868
Thermal Properties Metric English Comments
Melting Point 87.0 °C
189 °F
DSC; ASTM D3417- ISO 3146
Vicat Softening Point 68.0 °C
154 °F
ASTM D1525, ISO 306
Brittleness Temperature -100 °C
-148 °F
ASTM D746