Dow Retain® ABS 7490 ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Retain® ABS 7490 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM Data
Melt Flow 6.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.0 MPa
6240 psi
ASTM Data
Tensile Modulus 2.21 GPa
321 ksi
ASTM Data
Izod Impact, Notched 1.81 J/cm
3.39 ft-lb/in
ASTM Data
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Unannealed; ASTM Data
Vicat Softening Point 107 °C
225 °F