Material Notes:
FormulationNordel® IP 4520
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Mooney Viscosity 27

@Temperature 100 °C
27

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 9.50 MPa
1380 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 360 %
360 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00300 GPa
0.435 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.00790 GPa
1.15 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 27.9 kN/m
159 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 74 %

@Temperature 125 °C
74 %

@Temperature 257 °F
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
Thermal Properties Metric English Comments
Brittleness Temperature -44.0 °C
-47.2 °F
Temperature Retraction, TR-10