Mechanical Properties Metric English Comments
300% Modulus 0.00793 GPa
1.15 ksi
Measured on solution cast film from toluene; BAM 1245
Kraton® A1535 H (SEBS) Linear Triblock Copolymer
Description: Kraton A1535 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 57%. It is supplied from North America in the physical form ide..
300% Modulus 0.00790 GPa
1.15 ksi
ASTM D412
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..
300% Modulus 0.00790 GPa
1.15 ksi
DIN 53504
Lubrizol ESTANE® 58562 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00790 GPa
1.15 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4520 General Purpose Compound
FormulationNordel® IP 4520
300% Modulus 0.00790 GPa
1.15 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4570 Radiator/Heater Hose
FormulationNordel® IP 4570
300% Modulus 0.00790 GPa
1.15 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 5565 General Purpose Molding
FormulationNordel® IP 5565
300% Modulus 0.00790 GPa
1.15 ksi
DIN 53504
Lubrizol ESTANE® 54620 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..