Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00790 GPa | 1.15 ksi | ASTM D412 |
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
300% Modulus | 0.00790 GPa | 1.15 ksi | DIN 53504 |
Lubrizol ESTANE® 58562 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
300% Modulus | 0.00790 GPa | 1.15 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 General Purpose Compound FormulationNordel® IP 4520 |
|||
300% Modulus | 0.00790 GPa | 1.15 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 Radiator/Heater Hose FormulationNordel® IP 4570 |
|||
300% Modulus | 0.00790 GPa | 1.15 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 General Purpose Molding FormulationNordel® IP 5565 |
|||
300% Modulus | 0.00790 GPa | 1.15 ksi | DIN 53504 |
Lubrizol ESTANE® 54620 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |