Dow Corning® Class VI Elastomers are heat cured elastomer raw materials for use by customers fabricating medical devices and partsInformation provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Ultimate 8.20 MPa
1190 psi
Elongation at Break 830 %
830 %
Tear Strength 28.0 kN/m
160 pli