Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Multibase Multi-Flex® V 5502 TPE Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection Molding Features:Gloss, LowInformation provided by Multibase |
|||
Tear Strength | 28.0 kN/m | 160 pli | Split; ASTM D624 |
Northstar Polymers MSS-A70GQ High Performance Polyurethane Cast Elastomer System 70A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires cut/tear resistance, dry-abrasion resistance, slow resp.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 28 kN/m at 23°C. Value at 100°C is 13 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 73°F; ASTM D624 |
ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer with good fluid resistance, formulated to replace foamed thermoset elastomers such as EPDM and thermoplastic foams. It is polyolefin-based and desig.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Multibase Multi-Flex® A 5500 MR Natural TPE Thermoplastic Elastomer Information provided by Multibase |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 45-LR-9 TPE Product Description: StarTUFF TF 45-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Initial Tear Strength |
Saint-Gobain CHR® SG33-05(R) Industrial Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Initial Tear Strength |
Saint-Gobain CHR® SG35-05(R) Industrial Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Sumitomo Chemical ESPOLEX® 3675 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 3031-102 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3031-102 is specifically designe.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
ELASTO UK Dryflex® 502650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
ELASTO UK Dryflex® 650700 TPE, Improved Compression Set and High Temperature Resistance, 70A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Across Flow, Die C; ASTM D624 |
ExxonMobil Santoprene® 291-60B150 Thermoplastic Vulcanizate Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Diamond Polymers Softflex® SF 8900 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ISO 34-1 |
Alliance Polymers Viprene™ G50D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | B, cured 72 hrs @ RT |
ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | B, cured 72 hrs @ RT |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | |
Axiall 8740 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 38-096 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerOpaqueApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDisclai.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT38-034 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDi.. |