Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 28.0 kN/m | 160 pli | Split; ASTM D624 |
Northstar Polymers MSS-A70GQ High Performance Polyurethane Cast Elastomer System 70A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires cut/tear resistance, dry-abrasion resistance, slow resp.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 28 kN/m at 23°C. Value at 100°C is 13 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 28 kN/m at 23°C. Value at 100°C is 13 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 60ANS200 Thermoplastic Elastomer
(discontinued **) A soft, translucent thermoplastic elastomer (TPE) with a relative haze of 85 to 90%. This material is shear-dependent and can be processed on conventional thermoplastics equipment for injection mold.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 73°F; ASTM D624 |
ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer with good fluid resistance, formulated to replace foamed thermoset elastomers such as EPDM and thermoplastic foams. It is polyolefin-based and desig.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ XL-0153-79 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 80 EX Heat Cured Rubber - Extrusion Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-235 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 28.0 kN/m | 160 pli | Initial Tear Strength |
Saint-Gobain CHR® 2915-7 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Initial Tear Strength |
Saint-Gobain CHR® SG33-05(R) Industrial Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 6 High-Performance PTFE-Coated Glass Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C; ASTM D624 |
Teknor Apex Flexalloy® 9100-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Teknor Apex Uniprene® UN-7200-73 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Automotive Specifications: Chrysler MS-AK91; FORD WSS-M2D510-A7; .. |
|||
Tear Strength | 28.0 kN/m | 160 pli | M.D., Split Tear @ 254 mm/min; ASTM D1938 |
Eastman Embrace LV Copolyester for Shrink Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Diamond Polymers Softflex® SF 5596 Thermoplastic Elastomer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Diamond Polymers Softflex® SF 8900 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ISO 34-1 |
Alliance Polymers Viprene™ G50D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | B, cured 72 hrs @ RT |
ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | |
Axiall 8740 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Arlon T2040-B004 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide x 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyester Product: Cured Self-Fusing Silicone RubberCross-Section:.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 38-034M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDiscla.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ISO 34-B |
AlphaGary Evoprene™ 003 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 37-031 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Specialty Thermoplastic ElastomerMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® ST-6250 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |