Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 260 cSt | 260 cSt | kinetic/kinematic |
Dow Corning 193C Fluid Dow Corning ® 193C Fluid is a silicone glycol copolymer.Information provided by Dow Corning |
|||
Viscosity Measure | 260 cSt | 260 cSt | Kinetic/Kinematic |
Dow Corning DM6 Demulsifier Silicone polyether, acts as a performance booster for crude oil emulsion breakers.Information provided by Dow Corning |