Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Water Absorption 0.40 %
0.40 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 1.7 %
1.7 %
ASTM D 570(2)
Outgassing - Total Mass Loss 1.85 %
1.85 %
ASTM E595
Collected Volatile Condensable Material 0.00 %
0.00 %
ASTM E-595
Mechanical Properties Metric English Comments
Hardness, Rockwell E 80
80
ASTM D785
Hardness, Rockwell M 120
120
ASTM D785
Tensile Strength 138 MPa
20000 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Tensile Modulus 3.96 GPa
575 ksi
ASTM D638
Flexural Strength 165 MPa
24000 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Compressive Strength 165 MPa
24000 psi
10% Def.; ASTM D695
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Shear Strength 110 MPa
16000 psi
ASTM D732
Izod Impact, Notched 1.1 J/cm
2.0 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.35
0.35
dry vs. steel; QTM55007
K (wear) Factor >= 2010 x 10-8 mm³/N-M
>= 1000 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor applied; QTM 55010
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C

@Temperature -40.0 - 150 °C
17.0 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E831
Thermal Conductivity 0.259 W/m-K
1.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
ASTM D648
Glass Transition Temp, Tg 275 °C
527 °F
Amorphous; ASTM D3418
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+16 ohm
>= 1.00e+16 ohm
ASTM D257
Dielectric Constant 4.2

@Frequency 1e+6 Hz
4.2

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 23 kV/mm
580 kV/in
Short Term; ASTM D149
Dissipation Factor 0.026

@Frequency 1e+6 Hz
0.026

@Frequency 1e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Properties Metric English Comments
Ionic Impurities - Na (Sodium) 3.9 ppm
3.9 ppm
ICP/MS
Ionic Impurities - K (Potassium) 0.50 ppm
0.50 ppm
ICP/MS
Ionic Impurities - Fe (Iron) 1.5 ppm
1.5 ppm
ICP/MS
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable