Denka VINYKON W4023A PVC, W grade for equipment cords, for heat resistance

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka VINYKON W4023A PVC, W grade for equipment cords, for heat resistance.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.395 g/cc
0.05040 lb/in³
JIS-Z-8807
Deformation 7.0 %
7.0 %
JIS-K-6723
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
JIS-K-6301
Tensile Strength at Break 20.601 MPa
2987.9 psi
JIS-K-6723
Elongation at Break 330 %
330 %
JIS-K-6723
100% Modulus 0.013734 GPa
1.9920 ksi
JIS-A-5756
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -21.0 °C
-5.80 °F
JIS-K-6723
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+13 ohm-cm

@Temperature 60.0 °C
7.00e+13 ohm-cm

@Temperature 140 °F
JIS-K-6723
9.00e+14 ohm-cm

@Temperature 30.0 °C
9.00e+14 ohm-cm

@Temperature 86.0 °F
JIS-K-6723
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 86
JIS-A-5756
Heating: Retention Rate of Tensile Strength, % 98
JIS-A-5756
Oil Resistance: Retention of Tensile Strength, % 92
JIS-K-6723
Oil Resistance: Retention Rate of Elongation, % 90
JIS-K-6723
Thermostability, min, JIS-K-6723 >240