Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -21.0 °C | -5.80 °F | JIS-K-6723 |
Denka VINYKON M7300 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -21.0 °C | -5.80 °F | JIS-K-6723 |
Denka VINYKON W4023A PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -21.0 °C | -5.80 °F | DuPont Test Method |
DuPont Performance Polymers Kalrez® Spectrum™ 0090 Fluoroelastomer DuPont™ Kalrez® 0090 perfluoroelastomer parts deliver durable, reliable sealing solutions for applications requiring excellent rapid gas decompression (RGD) properties as well as high hardness and.. |