Westlake Plastics Lennite® CN-P UHMW Polyethylene (conductive)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Westlake Plastics
Trade Name Lennite® CN-P
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Westlake Plastics Lennite® CN-P UHMW Polyethylene (conductive).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Carbon-powder-filled, self-lubricating, conductive material with excellent abrasion-resistance and high impact strength. This material is light weight and easily machined, has good chemical and stress-crack resistance, and good wear-resistance. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 0.969 g/cc
0.0350 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength, Yield 39.3 MPa
5700 psi
ASTM D638
Elongation at Break 390 %
390 %
ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Dry; ASTM D257
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
Dry; ASTM D257