Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4701-15 Urethane Foam, Soft Seal PORON® 4701-15 Improved Soft Seal SeriesEnhanced Surface Toughness, Reliable Materials for Thinner DesignsIncreased Surface Toughness, Improved YieldsExcellent Compressibility and ConformabilityLon.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement. Standard available thickness 0.064"Features and Benefits of PORON Products: Excelle.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | Supporting Material; ASTM D1505 |
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Handheld Urethane Foam, Handheld Grade, PET Reinforced Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | supporting material; ASTM D1505 |
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | ISO 1183 |
Stir SpA SA 60 (PVC) Application: Extrusion pipe and profileInformation provided by STIR SpA |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | JIS-Z-8807 |
Denka VINYKON W4023A PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 306 Polyester Film, 300 Gauge Melinex® 306 is a clear, smooth pretreated polyester film. Melinex® 306 is produced from a lightly filled polymer, giving it a very smooth surface. The two side chemical coating provides adhesion .. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 606 Polyester Film, 300 Gauge Melinex® 606 is a very smooth two-side coated polyester film designed specifically for high density floppy disks.Also available in 285 GaugeInformation provided by DuPont. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge Melinex® XST6562 is a thermally stabilized high clarity polyester film with good handleability. It is pretreated on one film surface to promote adhesion.Information provided by DuPont. |
|||
Density | 1.395 g/cc | 0.05040 lb/in³ | ASTMD1505 |
DuPont Teijin Films Melinex® 6428 Polyester Film, 200 Gauge Melinex® 6428 is a high clarity polyester film. It is pretreated on both film surfaces to promote adhesion to EVA. Melinex® 6428 is a developmental film designed for the photovoltaics industry.Als.. |