DSM Arnite® TV6 241 SN PBT-GF20 FR(17)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® TV6 241 SN PBT-GF20 FR(17).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Glass Reinforced, Flame Retardant
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ISO 1183
Water Absorption 0.40 %
0.40 %
Sim. To ISO 62
Moisture Absorption 0.200 %
0.200 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 120 MPa
17400 psi
ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
ISO 527-1/-2
Tensile Modulus 8.50 GPa
1230 ksi
ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
22.2 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-1/-2
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.2

@Frequency 100 Hz
3.2

@Frequency 100 Hz
IEC 60250
3.2

@Frequency 1.00e+6 Hz
3.2

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
IEC 60250
0.014

@Frequency 1.00e+6 Hz
0.014

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 250 V
250 V
IEC 60112