Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Akulon® Fuel Lock FL-LP PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® Fuel Lock FL-LP PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low fuel permeation PA6 suitable for use in injection molding/welding of small engine fuel tanks, UV stabilized
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
dry; ISO 1183
Water Absorption 7.0 %
7.0 %
Sim. To ISO 62
Moisture Absorption 2.50 %
2.50 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
Tensile Modulus 1.80 GPa
261 ksi
dry; ISO 527-1/-2
Flexural Strength 65.0 MPa
9430 psi
dry; ISO 178
Flexural Modulus 1.60 GPa
232 ksi
dry; ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
cond; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
cond; ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
dry; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
cond; ISO 179/1eA
6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
dry; ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
dry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
dry; ISO 75-1/-2
Users viewing this material also viewed the following: