Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Asia Pacific) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S HSX (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1162T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1944 PC (Europe-Africa-Middle East) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LR180 PC (Europe-Africa-Middle East) LR180 is a medium viscosity, non UV, non release containing multipurpose polycarbonate recycle gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LR180R PC (Europe-Africa-Middle East) LR180R is a medium viscosity,release containing multipurpose polycarbonate industrial gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle .. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**) Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature -30.0 °C |
30.9 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature -20.0 °C |
30.9 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Borcoat™ EA165E Elastomer Modified Polypropylene for Extrusion Borcoat EA165E is an elastomer modified compound, based on a high molecular weight copolymer. The elastomer modification gives excellent low temperature impact resistance.Borcoat EA165E is recommen.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Akulon® Fuel Lock FL-LP PA6 Low fuel permeation PA6 suitable for use in injection molding/welding of small engine fuel tanks, UV stabilized |
|||
Charpy Impact, Notched | 6.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
30.9 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
30.9 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM EcoPaXX® Q-E7300 PA410-I Tube Extrusion |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |