Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cyclewood Solutions Xylomer™ XM1-KJD Injection Molding Compostable Resin

Category Polymer , Renewable/Recycled Polymer , Thermoplastic
Manufacturer Cyclewood Solutions
Trade Name Xylomer™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cyclewood Solutions Xylomer™ XM1-KJD Injection Molding Compostable Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
100% biodegradable and compostable thermoplastic. The compostable resin blend performs well compared to LDPE and is BPI certified compostable under ASTM D-6400. Xylomer™ is modified lignin, an abundant, natural byproduct of the paper manufacturing process, blended with other compostable polymers. Xylomer™ pellets have been demonstrated in injection molding and vacuum forming processes to create samples of cups and bowls.Information provided by Cyclewood Solutions.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Melt Flow 12.8 g/10 min

@Temperature 190 °C
12.8 g/10 min

@Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength 12.51 MPa
1815 psi
Elongation at Break 18.3 %
18.3 %
Flexural Modulus 0.496 GPa
72.0 ksi
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
Users viewing this material also viewed the following: