Material Notes:
Two component, silver-filled epoxy for hi-power applications. Cures with mild heat.
Physical Properties Metric English Comments
Viscosity 15000 cP
15000 cP
Thermal Properties Metric English Comments
Thermal Conductivity 7.20 W/m-K
50.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 232 °C
450 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.0020 ohm-cm
0.0020 ohm-cm
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 162 °C
0.167 hour

@Temperature 324 °F
Users viewing this material also viewed the following: