Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 7.20 W/m-K @Temperature 800 °C |
50.0 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
McDanel Advanced Ceramics AP 35 99% Alumina Information provided by McDanel Advanced Ceramic Technologies |
|||
Thermal Conductivity | 7.20 W/m-K | 50.0 BTU-in/hr-ft²-°F | |
Cotronics Duralco™ 120 500°F Silver Filled Epoxy, Electrically Conductive Contains over 70% ultra fine silver to provide excellent electrical conductivity. Cures at room temperature.>Applications: ideal for use where maximum conductivity is required. |
|||
Thermal Conductivity | 7.20 W/m-K | 50.0 BTU-in/hr-ft²-°F | |
Cotronics Duralco™ 124 650°F (340°C) Silver Filled Epoxy Two component, silver-filled epoxy for hi-power applications. Cures with mild heat. |
|||
Thermal Conductivity | 7.20 W/m-K | 50.0 BTU-in/hr-ft²-°F | |
Cotronics Duralco™ 126 450°F (230°C) Silver Filled Epoxy Two component, silver-filled epoxy for hi-power applications. Cures with mild heat. |