Thermal Properties Metric English Comments
Thermal Conductivity 7.20 W/m-K

@Temperature 800 °C
50.0 BTU-in/hr-ft²-°F

@Temperature 1470 °F
McDanel Advanced Ceramics AP 35 99% Alumina
Information provided by McDanel Advanced Ceramic Technologies
Thermal Conductivity 7.20 W/m-K
50.0 BTU-in/hr-ft²-°F
Cotronics Duralco™ 120 500°F Silver Filled Epoxy, Electrically Conductive
Contains over 70% ultra fine silver to provide excellent electrical conductivity. Cures at room temperature.>Applications: ideal for use where maximum conductivity is required.
Thermal Conductivity 7.20 W/m-K
50.0 BTU-in/hr-ft²-°F
Cotronics Duralco™ 124 650°F (340°C) Silver Filled Epoxy
Two component, silver-filled epoxy for hi-power applications. Cures with mild heat.
Thermal Conductivity 7.20 W/m-K
50.0 BTU-in/hr-ft²-°F
Cotronics Duralco™ 126 450°F (230°C) Silver Filled Epoxy
Two component, silver-filled epoxy for hi-power applications. Cures with mild heat.